Evaluation de l’inertie thermique du four a combustible petrole lampant atomise a la vapeur d’eau
Abstract
20s during firing operation of the charged chrged. In the same way a time-constant of 4h 36mn 06s is observed during the cooling of the empty kiln and 5h 33mn 17s during cooling of the charged kiln. That should help a better quality control of firing the ceramic products and allow other possible uses of the kiln.